通常在建筑工地的图颜色铝板,其性能是使它被广泛使用,但是也有一个好的外表,但着色过程中可能不是容易的颜色,这就要求员工及时检查观察问题的流程步骤。
Usually in the construction site, the drawing color aluminum plate, whose performance is to make it widely used, but also has a good appearance, but the coloring process may not be easy color, which requires employees to check and observe the process steps of the problem in time.
1.可能是由于阳极氧化膜厚度不足,需要检查阳极氧化过程是否规范,温度、电压、电导率等因素是否稳定。如有异常,应及时调整。
1. It may be due to the insufficient thickness of anodizing film, it is necessary to check whether the anodizing process is standardized, and whether the temperature, voltage, conductivity and other factors are stable. In case of any abnormality, it shall be adjusted in time.
2.也可能是由于染料溶液的pH值过高,可以用冰醋酸来调节pH值至标准值。
2. It may also be that the pH value of dye solution is too high, so glacial acetic acid can be used to adjust the pH value to the standard value.
3,或者因为颜色铝板氧化在水箱放置太久时间可以主张在这个时候及时染色但现状可以放置在阳极氧化槽或硝酸中和槽后适当的激活染色效果会很好。
3. Or because the color aluminum plate is oxidized in the water tank for too long, it can be claimed to dye in time at this time, but the current situation can be placed in the anodizing tank or nitric acid neutralization tank after the appropriate activation dyeing effect will be very good.
4.染料选择不当,染料已被分解或发霉需要更换合适的染料。
4. The dye is improperly selected, the dye has been decomposed or moldy, and the appropriate dye needs to be replaced.
5.氧化温度过低容易造成皮膜密度过高,可适当提高氧化温度。
5. If the oxidation temperature is too low, the density of the film will be too high, and the oxidation temperature can be increased properly.
如果彩色铝板不能着色的现象可以按照以上步骤进行检查,而且你不能随意改变方法,这样可能会导致颜色失效,不能使用浪费等情况。
If the color aluminum plate can't be colored, you can check according to the above steps, and you can't change the method at will, which may lead to color failure and waste.