铝板在生产过程中往往会有很多问题,铝板生产中为常见的问题不外乎表面问题、板型问题、轧制厚度问题。所以铝板生产厂家在铝板生产中要时刻的关注以上几个要点。
There are often many problems in the production of aluminum plate. The most common problems in the production of aluminum plate are surface problems, plate shape problems and rolling thickness problems. Therefore, aluminum plate manufacturers should always pay attention to the above points in aluminum plate production.
铝板生产中的表面问题:
Surface problems in aluminum plate production:
表面问题主要为擦划伤、黄油斑问题,铝板在生产过程中如果机台上面有金属颗粒那么会在生产过程中出现纹理一直的擦划伤,生产人员需要立即停机清理机台。黄油斑问题是由于轧制油没有及时更换或者是轧制设备的吹风系统出现故障导致的,虽然后期可通过铝板拉弯矫清洗进行处理,但是生产人员还是需要注意黄油斑,如果对于高要求的外观件对于黄油斑都是视为不合格的铝板。
The surface problems are mainly scratches and grease spots. If there are metal particles on the machine during the production process, the texture will be scratched all the time. The production personnel need to stop the machine immediately to clean the machine. The problem of grease spots is caused by the failure of the rolling oil or the failure of the blowing system of the rolling equipment. Although it can be treated by the cleaning of the aluminum plate in the later stage, the production personnel still need to pay attention to the yellow oil spots. If the appearance parts with high requirements are regarded as unqualified aluminum plates.
铝板生产中的板型问题:
Plate shape problems in aluminum plate production:
板型问题一直是比较难以控制的,主要和轧机轧辊有关系,轧机如果在长期轧制过程中没有及时修复轧辊磨损的间隙则会出现板型波浪问题,中浪和边浪都可能会产生。波浪板型问题已经发现生产人员需要立即向生产主任反馈,排除是否因为轧机压力不均匀还是其它原因,如果是轧辊磨损严重需要更换轧辊。
The plate shape problem has always been difficult to control, which is mainly related to the roll of the rolling mill. If the rolling mill fails to repair the worn gap of the roll in time during the long-term rolling process, the plate shape wave problem will occur, and both medium wave and side wave may occur. The wave plate shape problem has been found. The production personnel need to immediately feed back to the production director to rule out whether it is due to uneven rolling mill pressure or other reasons. If the roll is seriously worn, the roll needs to be replaced.
铝板生产中的厚度问题:
Thickness problems in aluminum plate production:
还是和轧机有关系,轧机压力不均匀导致,目前轧机都有在线测量设备,该问题已经不再经常出现。
It is still related to the rolling mill, which is caused by the uneven pressure of the rolling mill. At present, the rolling mill has on-line measuring equipment, and this problem is no longer frequent.
铝板硬度问题:
Hardness of aluminum plate:
主要和退火时间有关系,很多时候由于退火时间不足导致力学性能不达标,比如半硬状态的铝板出现折弯开裂,或者拉伸铝板出现拉伸开裂均是铝板硬度不达标,主要需要检查退火设备的温度、退火时间。
It is mainly related to the annealing time. In many cases, the mechanical properties are not up to the standard due to insufficient annealing time. For example, the bending cracking of semi-rigid aluminum plate or the tensile cracking of stretched aluminum plate are not up to the standard. It is mainly necessary to check the temperature and annealing time of the annealing equipment.
以上是铝板生产中的常见问题,本公司是一家铝板生产厂家,为用户提供优质铝板带产品,关注铝板质量,争创铝板。更多相关事项就来我们网站//www.renttoplux.com咨询了解吧!
The above are common problems in aluminum plate production. The company is an aluminum plate manufacturer, providing users with high-quality aluminum plate and strip products, paying attention to the quality of aluminum plate and striving to create an aluminum plate brand. For more information, please visit our website //www.renttoplux.com Consult and understand!